Determination of optimal carbon content on a particle size of LiFePO4/C cathode active nano-material for lithium-ion batteries

In order to optimize carbon content on LiFePO4/C particle size, three samples were synthesized by sol-gel method. The samples of LiFePO4/C were synthesized with the addition of 10, 30 and 50 % wt. of tartaric acid as a carbon precursor. All samples were characterized by XRD and SEM.

___

  • [1] H. Bih et al., J. Solid State Chem. 182, 821 (2009).
  • [2] A.A. Salah et al., Spectrochim. Acta Part A 65, 1007 (2006).
  • [3] G. Rousse et al., Solid State Sci. 4, 973 (2002).
  • [4] A.A. Salaha et al., J. Power Sources 140, 370 (2005).